Skip to main navigation Skip to search Skip to main content

Atomic layer deposition of ruthenium and ruthenium oxide thin films from a zero-valent (1,5-Hexadiene)(1-isopropyl-4-methylbenzene)ruthenium complex and o2

  • Hyo Jun Jung
  • , Jeong Hwan Han
  • , Eun Ae Jung
  • , Bo Keun Park
  • , Jin Ha Hwang
  • , Seung Uk Son
  • , Chang Gyoun Kim
  • , Taek Mo Chung
  • , Ki Seok An
  • Korea Research Institute of Chemical Technology
  • Hongik University
  • Sungkyunkwan University

Research output: Contribution to journalArticlepeer-review

53 Scopus citations

Abstract

Ruthenium (Ru) and ruthenium oxide (RuO2) thin films were grown by atomic layer deposition (ALD) using a novel zerovalent (1,5-hexadiene)(1-isopropyl-4-methylbenzene)Ru complex and O2 as the Ru precursor and oxidant, respectively. The self-limiting growth mode for the Ru and RuO2 ALD processes was achieved while varying the Ru precursor and O2 feeding time. Metallic Ru films were deposited at growth temperatures of 230-350 °C, while the temperature window for the growth of the RuO2 film was limited to <230 °C. At 270 °C, the growth per cycle (GPC) of Ru ALD was 0.076 nm/cycle, and the incubation times of Ru on SiO2 and TiN substrates were considerably short (3 cycles on SiO2, negligible on TiN) compared to that of Ru ALD from a high-valent Ru precursor and O2. The resistivity of the Ru film was as low as 29-36 μω·cm at growth temperatures of 270-350 °C. On the other hand, the RuO2 film was grown at a low temperature of 200 °C and showed a GPC of 0.15 nm/cycle with a resistivity of ∼270 μω·cm. In situ quadruple mass spectrometry analysis of the CO2 byproduct revealed that the amount of subsurface oxygen extracted during the Ru pulse half-cycle affected the resultant film phase, either Ru or RuO2, which was strongly influenced by the growth temperature.

Original languageEnglish
Pages (from-to)7083-7090
Number of pages8
JournalChemistry of Materials
Volume26
Issue number24
DOIs
StatePublished - 23 Dec 2014

Fingerprint

Dive into the research topics of 'Atomic layer deposition of ruthenium and ruthenium oxide thin films from a zero-valent (1,5-Hexadiene)(1-isopropyl-4-methylbenzene)ruthenium complex and o2'. Together they form a unique fingerprint.

Cite this