TY - JOUR
T1 - Birefringence characteristics of PET-based copolymers in an injection molded specimen
AU - Jeoung, Young Hyun
AU - Lyu, Min Young
N1 - Publisher Copyright:
© The Author(s) 2026
PY - 2026
Y1 - 2026
N2 - The optical anisotropy of transparent injection-molded poly (ethylene terephthalate) (PET)-based copolyesters, including a biomass-derived PET copolymer, was investigated through birefringence and retardation measurements. Injection molding simulation was also performed to predict residual stress distributions. The effects of molding conditions and copolymer composition on optical anisotropy were systematically evaluated. The average retardation decreased from 468.6 to 190.3 nm as the injection temperature increased from 260 to 280°C, whereas it increased from 226.6 to 347.6 nm as the packing pressure increased from 40 to 80 MPa. Birefringence increased in the order of PET, poly (ethylene terephthalate-co-1,4-cyclohexanedimethylene terephthalate) (PETG), poly (cyclohexanedimethylene terephthalate-co-ethylene terephthalate) (PCTG), and poly (ethylene terephthalate-co-isosorbide terephthalate-co-cyclohexanedimethylene terephthalate) (PEICT). Increasing the 1,4-cyclohexanedimethanol (CHDM) content increased birefringence, while the incorporation of isosorbide (ISB) further enhanced birefringence by restricting polymer chain mobility and stress relaxation during cooling. These results demonstrate that the optical anisotropy of transparent PET-based copolyesters can be effectively controlled through copolymer composition and injection molding conditions.
AB - The optical anisotropy of transparent injection-molded poly (ethylene terephthalate) (PET)-based copolyesters, including a biomass-derived PET copolymer, was investigated through birefringence and retardation measurements. Injection molding simulation was also performed to predict residual stress distributions. The effects of molding conditions and copolymer composition on optical anisotropy were systematically evaluated. The average retardation decreased from 468.6 to 190.3 nm as the injection temperature increased from 260 to 280°C, whereas it increased from 226.6 to 347.6 nm as the packing pressure increased from 40 to 80 MPa. Birefringence increased in the order of PET, poly (ethylene terephthalate-co-1,4-cyclohexanedimethylene terephthalate) (PETG), poly (cyclohexanedimethylene terephthalate-co-ethylene terephthalate) (PCTG), and poly (ethylene terephthalate-co-isosorbide terephthalate-co-cyclohexanedimethylene terephthalate) (PEICT). Increasing the 1,4-cyclohexanedimethanol (CHDM) content increased birefringence, while the incorporation of isosorbide (ISB) further enhanced birefringence by restricting polymer chain mobility and stress relaxation during cooling. These results demonstrate that the optical anisotropy of transparent PET-based copolyesters can be effectively controlled through copolymer composition and injection molding conditions.
KW - biomass-PET
KW - birefringence
KW - injection molding
KW - PET-based copolymers
KW - residual stress
KW - retardation
UR - https://www.scopus.com/pages/publications/105049335856
U2 - 10.1177/07316844261484671
DO - 10.1177/07316844261484671
M3 - Article
AN - SCOPUS:105049335856
SN - 0731-6844
JO - Journal of Reinforced Plastics and Composites
JF - Journal of Reinforced Plastics and Composites
ER -