T1 - Effect of Strain Aging on Tensile Behavior and Properties of API X60, X70, and X80 Pipeline Steels
AU - Lee, Sang In
AU - Lee, Seung Yong
AU - Lee, Seok Gyu
AU - Jung, Hwan Gyo
AU - Hwang, Byoungchul
N1 - Publisher Copyright:
© 2018, The Korean Institute of Metals and Materials.
PY - 2018/11/1
Y1 - 2018/11/1
N2 - The effect of strain aging on tensile behavior and properties of API X60, X70, and X80 pipeline steels was investigated in this study. The API X60, X70, and X80 pipeline steels were fabricated by varying alloying elements and thermomechanical processing conditions. Although all the steels exhibited complex microstructure consisting of polygonal ferrite (PF), acicular ferrite, granular bainite (GB), bainitic ferrite (BF), and secondary phases, they had different fractions of microstructures depending on the alloying elements and thermomechanical processing conditions. The tensile test results revealed that yielding behavior steadily changed from continuous-type to discontinuous-type as aging temperature increases after 1% pre-strain. After pre-strain and thermal aging treatment in all the steels, the yield and tensile strengths, and yield ratio were increased, while the uniform elongation and work hardening exponent were decreased. In the case of the X80 steel, particularly, the decrease in uniform elongation was relatively small due to many mobile dislocations in PF, and the increase in yield ratio was the lowest because a large amount of harder microstructures such as GB, BF, and coarse secondary phases effectively enhanced work hardening.
AB - The effect of strain aging on tensile behavior and properties of API X60, X70, and X80 pipeline steels was investigated in this study. The API X60, X70, and X80 pipeline steels were fabricated by varying alloying elements and thermomechanical processing conditions. Although all the steels exhibited complex microstructure consisting of polygonal ferrite (PF), acicular ferrite, granular bainite (GB), bainitic ferrite (BF), and secondary phases, they had different fractions of microstructures depending on the alloying elements and thermomechanical processing conditions. The tensile test results revealed that yielding behavior steadily changed from continuous-type to discontinuous-type as aging temperature increases after 1% pre-strain. After pre-strain and thermal aging treatment in all the steels, the yield and tensile strengths, and yield ratio were increased, while the uniform elongation and work hardening exponent were decreased. In the case of the X80 steel, particularly, the decrease in uniform elongation was relatively small due to many mobile dislocations in PF, and the increase in yield ratio was the lowest because a large amount of harder microstructures such as GB, BF, and coarse secondary phases effectively enhanced work hardening.
KW - API pipeline steels
KW - High deformability
KW - Strain aging
KW - Tensile properties
KW - Yielding behavior
UR - http://www.scopus.com/inward/record.url?scp=85051656079&partnerID=8YFLogxK
U2 - 10.1007/s12540-018-0173-9
DO - 10.1007/s12540-018-0173-9
M3 - Article
AN - SCOPUS:85051656079
SN - 1598-9623
VL - 24
SP - 1221
EP - 1231
JO - Metals and Materials International
JF - Metals and Materials International
IS - 6
ER -